| Composición de materiales: | 80% Meta Aramida + 20% Para Aramida | Peso: | 70-90 G/M |
|---|---|---|---|
| Ancho: | 150cm | Después del tiempo de brillo: | 0.8s |
| longitud dañada: | 4,5 cm | Proceso: | no tejido perforado con aguja |
| Resaltar: | 4.5 Cm Damaged Length Aramid Felt,0.8s After Glow Time Aramid Felt,70-90 gsm Meta Aramid Felt |
||
Aramid Needle Punched Felt Item: Aramid Felt Width: 150 cm Weight: 70–90 gsm Composition: 80% Meta Aramid + 20% Para Aramid Process: Needle punched nonwoven Description This aramid felt is manufactured by needle punching process, blended with 80% meta-aramid and 20% para-aramid staple fiber. Meta-aramid provides excellent inherent flame retardancy and thermal stability, while para-aramid brings outstanding tensile strength and tear resistance. The material will not melt or